H. Razavizadeh, ERSHAD-LANGROUDI A.. THE LEACHING OF NEZAMABAD SCHEELITE WITH SULFURIC ACID. IJMSE 2004; 1 (1) :9-15
URL: http://ijmse.iust.ac.ir/article-1-92-en.html
Abstract:   (34563 Views)
A new process for recovering scheelite ores comprises producing a concentrate from the ore, then leaching the concentrate with H_2SO_4 in the presence of H_3PO_4 and Na Cl at atmosphericpressure are discussed. Finely purification of the product will be described. The amounts of dissolution of tungsten in acid depend on the parameters such as time, temperature, type and concentration of acid and stilt as well as solid-liquid reaction. These factors were optimized for the result and described in details.
     
Type of Study: Research Paper | Subject: Ceramics

Add your comments about this article : Your username or Email:
CAPTCHA

Send email to the article author


Rights and permissions
Creative Commons License This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License.

© 2022 All Rights Reserved | Iranian Journal of Materials Science and Engineering

Designed & Developed by : Yektaweb