Eftekhari Yekta B, Honarvar S. EFFECT OF TiO2 ADDITION ON BONDING STRENGTH OF CaO-P2O5 Na2O-TiO2 BIOACTIVE GLASS CERAMIC COATING. IJMSE 2014; 11 (4) :1-7
URL: http://ijmse.iust.ac.ir/article-1-714-en.html
Abstract:   (19077 Views)
The effect of titanium dioxide addition on bonding strength of CaO-P2O5 -Na 2O-TiO2glass-ceramic system was investigated as a coating on titanium substrate. Thus, different amounts of TiO2 (2, 3.5 and 5mol %) were added to the base glass batch composition. The prepared glaze slips were applied on the substrate by dip coating method, dried and then heat treated at various temperatures. After that, bonding strength of the glass- substrates was determined via shear stress testing method. The de-bonded interfaces were analyzed by scanning electron microscopy (SEM). According to these results, the 5 mol% TiO 2 containing coating showed the best bonding strength, comparing with the other coatings. The bioactivity of the coated samples was investigated by soaking them in simulated body fluid (SBF). The surface of the samples was studied using SEM and X-Ray microprobe and it was observed that an apatite layer was grown on their surface
Full-Text [PDF 5285 kb]   (5409 Downloads)    
Type of Study: Research Paper |

Add your comments about this article : Your username or Email:
CAPTCHA

Send email to the article author


Rights and permissions
Creative Commons License This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License.

© 2022 All Rights Reserved | Iranian Journal of Materials Science and Engineering

Designed & Developed by : Yektaweb